| 廠家及牌號 | 試驗條件 | 測試方法 | 裝有測量儀表的落鏢沖擊 |
| PPO(PPE) 沙伯基礎(chǔ) NORYL GTX™ GTX626 resin (高耐熱性,耐化學(xué)性良好,擠出吹塑成型) | -30°C,EnergyatPeakLoad | ASTMD3763 | 36.6 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL PPX™ PPX630 resin | -30°C,TotalEnergy | ASTMD3763 | 20.4 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL™ PPX640 resin (延高的拉伸率,高剛性注射成型填料:玻璃纖維增強材料, 40% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 14.1 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL PPX™ PPX830 resin | -30°C,TotalEnergy | ASTMD3763 | 10.0 J |
| 該文獻版權(quán)所有-請勿轉(zhuǎn)載或-其它用途.http://m.melanomaexpert.com/ | |||
| PPO(PPE) 沙伯基礎(chǔ) NORYL GTX™ GTX902 resin (耐化學(xué)性良好,可噴涂的,注射成型) | -40°C,EnergyatPeakLoad | ASTMD3763 | 19.7 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL PPX™ PPX640F resin (延高的拉伸率,高剛性注射成型填料:玻璃纖維增強材料, 40% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 14.1 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL™ WCV065 resin (良好的柔韌性,無鹵,阻燃性,擠出涂層) | -30°C,TotalEnergy | ASTMD3763 | 42.0 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL™ SE100X resin | -30°C,EnergyatPeakLoad | ASTMD3763 | 16.3 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL™ EZ250 resin (可加工性良好,耐化學(xué)性良好,注射成型) | -40°C,EnergyatPeakLoad | ASTMD3763 | 33.9 J |
| PPO(PPE) 沙伯基礎(chǔ) NORYL PPX™ PPX630F resin (高剛性,延高的拉伸率,注射成型填料:玻璃纖維增強材料, 30% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 20.4 J |
| 溫馨提示 | |||