| 廠家及牌號(hào) | 試驗(yàn)條件 | 測(cè)試方法 | 熔流率(熔體流動(dòng)速率)(260°C/5.0kg) |
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL PPX™ PPX7110 resin | ASTMD1238 | 11 g/10min | |
| PPO(PPE)+PS 沙伯基礎(chǔ) LNP™ LUBRICOMP™ Noryl_NWR5810 compound | ASTMD1238 | 5.5 g/10min | |
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL™ RN0401 resin | ASTMD1238 | 30 g/10min | |
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL™ PPX640 resin (延高的拉伸率,高剛性注射成型填料:玻璃纖維增強(qiáng)材料, 40% 填料按重量。) | ASTMD1238 | 1.3 g/10min | |
| 該文獻(xiàn)版權(quán)所有.請(qǐng)勿.轉(zhuǎn)載或其它用途.http://m.melanomaexpert.com/ | |||
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL PPX™ PPX630 resin | ASTMD1238 | 2.6 g/10min | |
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL PPX™ PPX630F resin (高剛性,延高的拉伸率,注射成型填料:玻璃纖維增強(qiáng)材料, 30% 填料按重量。) | ASTMD1238 | 2.6 g/10min | |
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL PPX™ PPX7200 resin | ASTMD1238 | 16 g/10min | |
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL PPX™ PPX640F resin (延高的拉伸率,高剛性注射成型填料:玻璃纖維增強(qiáng)材料, 40% 填料按重量。) | ASTMD1238 | 1.3 g/10min | |
| PPO(PPE)+PS Generic Generic PPE+PS+PP | ASTMD1238 | 11到16 g/10min | |
| PPO(PPE)+PS 沙伯基礎(chǔ) NORYL PPX™ PPX7115F resin (抗撞擊性高,高耐熱性,注射成型) | ASTMD1238 | 14 g/10min | |
| 溫馨提示 | |||
| 1.有關(guān)“熔流率(熔體流動(dòng)速率)(260°C/5.0kg) PPO(PPE)+PS”類數(shù)據(jù)資訊最多展示10條.更多牌號(hào)應(yīng)用數(shù)據(jù)請(qǐng)向客服索取。 2.有關(guān)“PPO(PPE)+PS塑料原料價(jià)格”類數(shù)據(jù)的實(shí)時(shí)性及更多塑料原料價(jià)格行情敬請(qǐng)關(guān)注我們的資訊動(dòng)態(tài). | |||
● PS 無(wú)缺口懸臂梁沖擊(23°C)
● PS 光澤度(60°)
● HIPS UL 阻燃等級(jí)
● PUR-MDI 維卡軟化溫度
● PA+PPO(PPE) 載荷下熱變形溫度(1.8MPa,未退火,3.18mm)